PTFE Creep and Cold Flow: Causes, Data & How to Reduce Deformation

PTFE creep is gradual, time-dependent deformation under sustained stress, even when the applied load does not change. The amount depends on stress, temperature, loading time, material grade, component geometry and mechanical restraint. In a gasket it can reduce sealing pressure; in a bushing it can alter clearance. Better material selection and design can reduce deformation, but no PTFE grade is completely free of creep.

What Is PTFE Creep and Cold Flow?

Creep is the increase in strain that develops while a material remains under sustained stress. In PTFE engineering, cold flow is commonly used for the same time-dependent behavior, particularly when it occurs near room temperature. The terms are not separate failure modes, although cold flow often emphasizes visible movement or loss of shape under pressure.

Thermal expansion is different: dimensions change because temperature changes, whether or not the part carries a load. Stress relaxation describes the other side of time-dependent behavior. Under approximately constant strain, such as a gasket held between bolted flanges, the stress needed to maintain that strain falls with time. Under constant stress, creep is observed as increasing deformation.

Diagram showing immediate and time-dependent PTFE deformation under sustained load.

Why Does PTFE Creep Under Load?

PTFE has a lower stiffness than many structural plastics and metals. Under sustained stress, its molecular structure can rearrange gradually, so deformation continues after the immediate elastic response. Low friction does not prevent this: friction describes interaction at a sliding surface, while creep resistance describes the bulk material’s ability to retain shape under load.

Five variables deserve attention. Higher stress generally produces more deformation. Higher temperature increases molecular mobility. Longer loading allows more time-dependent strain to develop. Virgin and filled grades behave differently, but performance depends on the complete formulation and processing history. Geometry also changes the local stress: thin walls, sharp transitions, unsupported spans and wide extrusion gaps can concentrate load, while a surrounding housing or backup ring may restrain movement.

This is why a short tensile-strength value or room-temperature hardness number cannot predict PTFE creep under load. The relevant data must match the grade, stress mode, temperature and intended service time.

How Much Does PTFE Deform Over Time?

The Teflon™ PTFE Properties Handbook gives a worked compression example at 23°C (73°F) and 6.9 MPa (1,000 psi).

Loading pointTemperatureCompressive stressTotal strainApparent modulusData status
Initial response23°C (73°F)6.9 MPa (1,000 psi)0.015 in/in (1.5%)66,700 psiShort-term value from the handbook’s stress-strain curve
After 200 hours23°C (73°F)6.9 MPa (1,000 psi)0.020 in/in (2.0%)50,000 psiReported from the time-under-load curve; includes initial and time-dependent strain
After 1 year23°C (73°F)6.9 MPa (1,000 psi)0.025 in/in (2.5%)40,000 psiExtrapolated from the curve, not a measured one-year result

For scale, 2.0% strain corresponds to 0.40 mm of total compression in a 20 mm section while held under the stated load. That calculation does not predict recovery after unloading, and it does not establish a universal design allowance. It shows why an unloaded part can pass dimensional inspection yet change enough in service to affect contact pressure or a close fit. Drawing tolerances should therefore be reviewed alongside load and restraint, not separately; our guide to PTFE machining tolerances explains the manufacturing side of that review.

How Creep Affects PTFE Seals, Gaskets, Bushings and Valve Seats

ComponentPotential creep-related problemWhat engineers should evaluate
PTFE gasketsThickness reduction, stress relaxation and loss of sealing pressureGrade, thickness, flange restraint, surface condition and bolt load
PTFE valve seatsChanged contact geometry, extrusion or leakageSeat profile, pressure, temperature, backing support and extrusion path
PTFE bushingsBore distortion, alignment change or loss of designed clearanceProjected bearing pressure, housing support, motion, mating shaft and grade
Custom PTFE sealsLoss of preload or movement into an extrusion gapGland geometry, gap size, backup support and pressure-temperature cycles
Custom machined PTFE partsLong-term dimensional drift at loaded featuresWall thickness, load path, restraint, acceptable strain and inspection condition

In a bolted gasket joint, flange position is largely constrained. As the PTFE changes thickness, the clamping stress can fall, reducing sealing force even if the bolts have not visibly moved. A bushing behaves differently: radial load and housing support can change the bore shape and running clearance. The direction and magnitude of change depend on the assembly, so don’t treat clearance as a machining-only question.

Bolted flange cross-section showing PTFE gasket stress relaxation and reduced sealing pressure

How to Reduce PTFE Creep

Select the formulation around the application. Virgin PTFE may be required for purity, chemical resistance, or electrical performance, while an appropriately selected filled or modified grade may resist deformation better. Glass, carbon and bronze fillers do not produce the same result, and each can change wear, friction, chemical compatibility, electrical behavior, density and machinability. Use grade-specific data rather than assuming that a higher filler percentage is automatically better. Our virgin vs filled PTFE guide covers the main selection trade-offs.

Reduce and redistribute stress. Increase the effective bearing area where practical, remove point loads, support thin sections and limit extrusion gaps. A housing, shoulder, metal backup ring or other mating feature can restrain PTFE without asking the polymer to carry the full structural load. For gaskets, thickness and flange condition should be selected together rather than adding material as a default safety measure.

Verify the design at service conditions. Review creep or stress-relaxation data for the specified grade at the relevant temperature, stress and duration. Where failure would be costly, test the component or assembly and define whether measurements are taken under load, immediately after unloading or after a recovery period. If the required stiffness or dimensional stability still cannot be reached, compare another engineering polymer or a supported composite design instead of forcing PTFE into a structural role.

Engineering check: Before releasing a sustained-load PTFE part, document the material grade, load direction, calculated contact or bearing stress, temperature range, loading duration, mechanical restraint, allowable deformation and inspection condition.
Need a custom PTFE component for a sustained-load application?

At Golden Collar, we machine PTFE components from customer drawings. Send us the drawing, proposed grade, critical dimensions, load, temperature and expected service time through our request-a-quote page so we can review the manufacturing and material requirements with you.

FAQs

Can annealing a machined PTFE part prevent creep?

No. Annealing may reduce residual stress and dimensional movement associated with stock production or machining, but it does not remove PTFE’s time-dependent deformation under service load. Grade selection, geometry, support, temperature and sustained stress still control creep performance.

PTFE can recover part of the deformation after unloading, and recovery may continue with time. Full and immediate recovery should not be assumed, especially after high strain, elevated temperature or long loading. Inspection requirements should state how long the part rests before measurement.

It can support the design when the model uses grade-specific, time- and temperature-dependent material data with realistic contact and restraint conditions. A simple linear-elastic static model predicts immediate deformation, not long-term creep. Results should be checked against published data or physical testing.

There is no universal retightening rule. The safe procedure depends on the gasket construction, flange system, process fluid, temperature and equipment requirements. Follow the engineered assembly procedure, and never retighten a hot or pressurized joint unless an approved procedure specifically permits it.

No. A tighter tolerance controls the starting dimension but does not stop time-dependent strain in service. The drawing should separate manufacturing tolerance from allowable in-service deformation and define the load, temperature, restraint and measurement condition used to evaluate the finished assembly.

Share:

After reading the article, if you want to understand or buy PTFE products, please click on the right to contact us, we have professional engineers to contact you

Loading latest posts...
Shopping Cart
Scroll to Top